Experimental Study on Volatilization of TRIS(77-86-1) in the Process of Energy Storage

The volatility of the monovalent, binary and ternary systems composed of neopentyl glycol, pentaerythritol and TRIS(77-86-1) in solid-solid phase transition and solid-liquid phase transition was studied. In the process, the weight loss rate is low, within 5%, the material sealed after the loss of weight phenomenon; in the solid-liquid transition, the weight loss rate is large, after sealing a slight weight loss. The higher the temperature, the greater the volatile polyol. The different composition of the polyol system in the energy storage process have different degrees of weight loss in the use of materials should be considered the seal, so as not to affect the thermal performance.

 

 